Yayın:
Assessment of color strength and color difference values of polyester fabrics containing continuous weft yarns after abrasion

dc.contributor.buuauthorAkgün, Mine
dc.contributor.buuauthorBecerir, Behçet
dc.contributor.buuauthorAlpay, Halil Rıfat
dc.contributor.departmentMühendislik Fakültesi
dc.contributor.departmentTekstil Mühendisliği Bölümü
dc.contributor.orcid0000-0002-2655-2773
dc.contributor.researcheridAAG-9756-2021
dc.contributor.researcheridAAH-1445-2021
dc.contributor.scopusid9839293900
dc.contributor.scopusid9839809500
dc.contributor.scopusid9841273700
dc.date.accessioned2022-10-31T08:02:43Z
dc.date.available2022-10-31T08:02:43Z
dc.date.issued2007-08-22
dc.description.abstractThis paper assesses the color difference and color strength values (K/S) obtained for eight disperse-dyed polyester fabric samples with different fabric construction parameters (weft yam type, weft yam count, weft density and fabric weave) after four sets of abrasion cycles. Warp yarn type and count, warp density, and warp yam twist are the same for all fabrics. Fabric samples are dyed in a commercial red disperse dye (C.I. Disperse Red 74:1) and four different abrasion cycles (2500, 5000, 7500, 10000) are used. The KISS values of the abraided fabrics and color difference values between the control fabric (dyed but not abraided) and abraded fabrics are calculated. The main differences in the KISS and color difference values are observed between 0-2500 abrasion cycles. The high tenacity of the polyester fibers and continuous polyester yams causes some fuzz but no pilling formation on the fabric surface that lead to increased K/S values and color differences. Fiber dullness, yam thickness, yam density and fabric weave are concluded to have different effects on the appearance after abrasion.
dc.identifier.citationAkgün, M. vd. (2007). "Assessment of color strength and color difference values of polyester fabrics containing continuous weft yarns after abrasion". Fibers and Polymers, 8(5), 495-500.
dc.identifier.doi10.1007/BF02875871
dc.identifier.endpage500
dc.identifier.issn1229-9197
dc.identifier.issue5
dc.identifier.scopus2-s2.0-36749059483
dc.identifier.startpage495
dc.identifier.urihttps://doi.org/10.1007/BF02875871
dc.identifier.urihttps://link.springer.com/article/10.1007%2FBF02875871
dc.identifier.urihttp://hdl.handle.net/11452/29269
dc.identifier.volume8
dc.identifier.wos000250801900008
dc.language.isoen
dc.publisherKorean Fiber Society
dc.relation.journalFibers and Polymers
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi
dc.rightsinfo:eu-repo/semantics/closedAccess
dc.subjectAbrasion
dc.subjectColor
dc.subjectColor strength
dc.subjectDisperse dyes
dc.subjectPolyester
dc.subjectMaterials science
dc.subjectPolymer science
dc.subjectWool/polyester blended fabrics
dc.subjectVarying structural parameters
dc.subjectSingle-fiber transfer
dc.subjectRing spun yarns
dc.subjectCotton fabrics
dc.subjectOpen-end
dc.subjectPerformance
dc.subjectReflectance
dc.subjectResistance
dc.subjectWool
dc.subject.scopusWeft; Yarn Count; Carbon Fiber
dc.subject.wosMaterials science, textiles
dc.subject.wosPolymer science
dc.titleAssessment of color strength and color difference values of polyester fabrics containing continuous weft yarns after abrasion
dc.typeArticle
dc.wos.quartileQ2 (Materials science, textiles)
dc.wos.quartileQ3 (Polymer science)
dspace.entity.typePublication
local.contributor.departmentMühendislik Fakültesi/Tekstil Mühendisliği Bölümü
local.indexed.atScopus
local.indexed.atPubMed
local.indexed.atWOS

Dosyalar

Lisanslı seri

Şimdi gösteriliyor 1 - 1 / 1
Placeholder
Ad:
license.txt
Boyut:
1.71 KB
Format:
Item-specific license agreed upon to submission
Açıklama