An investigation on microstructure and mechanical properties of post-weld heat-treated friction stir welds in aluminum alloy 2024-W

dc.contributor.authorDurgun, İsmail
dc.contributor.buuauthorAydın, Hakan
dc.contributor.buuauthorBayram, Ali
dc.contributor.departmentMühendislik Fakültesi
dc.contributor.departmentMakine Mühendisliği Bölümü
dc.contributor.scopusid16312009400
dc.contributor.scopusid7004197848
dc.date.accessioned2023-05-23T12:29:09Z
dc.date.available2023-05-23T12:29:09Z
dc.date.issued2013
dc.description.abstractThe present work describes the results obtained from microstructural and mechanical evaluation of post-weld heat treated friction stir welds of 2024 aluminum alloys in the W temper state. Post-weld heat treatments have been carried out at 510 degrees C for 2.5 h followed by ageing at room temperature for 6 months, at 100 degrees C and 190 degrees C for 10 h, and by cooling in static air (O-temper). The solution treatment caused abnormal coarsening of the grains in the stir zone, which resulted in a drop in microhardness. The strength of the as-welded joint was significantly incrased by post weld heat treatments. The maximum hardness and strength values were obtained in T6 (190 degrees C, 10 h) treated joint. However, the T6 (190 degrees C, 10 h) treated joint had the lowest ductility. On the other hand, the tensile properties of the post-weld heat treated joints were far lower than those of the unwelded base materials in the same temper states. In addition, the post-weld heat treatments did not significantly change the fracture locations of the friction stir welds.
dc.identifier.citationAydın, H. vd. (2013). “An investigation on microstructure and mechanical properties of post-weld heat-treated friction stir welds in aluminum alloy 2024-W”. Proceedings of the Institution of Mechanical Engineers, Part C- Journal of Mechanical Engineering Science, 227(C4), 649-662.
dc.identifier.endpage662
dc.identifier.issn0954-4062
dc.identifier.issn2041-2983
dc.identifier.issueC4
dc.identifier.scopus2-s2.0-84880772926
dc.identifier.startpage649
dc.identifier.urihttps://doi.org/10.1177/0954406212452479
dc.identifier.urihttp://hdl.handle.net/11452/32749
dc.identifier.volume227
dc.identifier.wos000316757900001
dc.indexed.wosSCIE
dc.language.isoen
dc.publisherSage Publication
dc.relation.collaborationSanayi
dc.relation.journalProceedings of the Institution of Mechanical Engineers, Part C-Journal of Mechanical Engineering Science
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi
dc.rightsinfo:eu-repo/semantics/closedAccess
dc.subjectEngineering
dc.subjectPost-weld heat treatment
dc.subjectFriction stir welding
dc.subject2024 aluminum alloy
dc.subjectMechanical properties
dc.subjectTensile properties
dc.subjectFracture locations
dc.subjectMg alloys
dc.subjectJoints
dc.subjectBehavior
dc.subjectFatigue
dc.subjectParameters
dc.subjectAA2024
dc.subjectHeat treatment
dc.subjectMechanical properties
dc.subjectWelds
dc.subject2024 aluminum alloy
dc.subjectFracture location
dc.subjectMechanical evaluation
dc.subjectMicrostructure and mechanical properties
dc.subjectPost weld heat treatment
dc.subjectPost-weld heat treated
dc.subjectPost-weld heat treated joints
dc.subjectSolution treatments
dc.subjectFriction stir welding
dc.subject.scopusAluminum; Bobbins; Welded Joints
dc.subject.wosEngineering, mechanical
dc.titleAn investigation on microstructure and mechanical properties of post-weld heat-treated friction stir welds in aluminum alloy 2024-W
dc.typeArticle
dc.wos.quartileQ3
dspace.entity.typePublication
local.contributor.departmentMühendislik Fakültesi/Makine Mühendisliği Bölümü
local.indexed.atScopus
local.indexed.atWOS

Files

License bundle

Now showing 1 - 1 of 1
Placeholder
Name:
license.txt
Size:
1.71 KB
Format:
Item-specific license agreed upon to submission
Description: